PR-UM-PFIR-A-10

Geometry
Rectangular
Tip Radius (nm)
Nom: 20.0
Max: 35.0
Frequency (KHz)
Nom: 150
Min: 90
Max: 210
Length (µm)
Nom: 125
Min: 115
Max: 135
Spring Const (N/m)
Nom: 5.0
Min: 1.5
Max: 10.0
Width (µm)
Nom: 35
Min: 33
Max: 37
Price: $420.00 (USD)
Sold in packs of 10
+
-
Questions? Free, Online Consulting
Overview

A 10 pack of probes for PeakForce Tapping mode imaging and nanoIR spectroscopic measurements. Unmounted for use on Bruker's IconIR system or others systems that can take a standard cantilever chip.


This 150khz tapping mode probe has a full wrap gold coating, on the reflex side — for increased feedback laser signal, on the tip side   to enable nanoIR measurements.

Tip Specification
PR-UM-PFIR-A-10 Tip Image
Au tip side coating on the cantilever and pyramidal tip specifically to enable nanoIR measurements.
Tip Height (h): 12.5 µm
Front Angle (FA): 17.5º
Back Angle (BA): 25.0º
Side Angle (SA): 20.0º
Cantilever Specification
PR-UM-PFIR-A-10 Cantilever Image
Au reflex coating on the backside of the cantilever increases the feedback laser signal on the photodetector.
Material: 0.010-0.025Ohmcm Antimony (n) doped Si.
Geometry: Rectangular
Cantilevers Number: 1
Cantilever Thickness (Nom): 1.75µm
Back Side Coating: Au 50 nm